2.Performance :
Slightly increased life and sparkability due to the addition of 0.8% zirconium oxide.
Balls up easily in AC applications. Handles higher current with less splitting. Improved arc starts and arc stability. Offers minimal tungsten contamination.
DESIGNATION | COMPOSITION | IMPURITIES% | TUNGSTEN% | COLOR MARK |
DIOXIDE | OXIDE IN% |
WZr8 | Zro2 | 0.70-0.90 | <0.2 | REMAINDER | WHITE |
Designation | Composition Dioxide | Oxide in% | Impurities Content % | Tungsten Content% | Color Mark | WL10 | LA2O3 | 0.80~1.20 | <0.2 | Remainder | tungsten | WL15 | LA2O3 | 1.30~1.70 | <0.2 | Remainder | tungsten | WL20 | LA2O3 | 1.80~2.20 | <0.2 | Remainder | tungsten | WT20 | ThO2 | 1.70~2.20 | <0.2 | Remainder | tungsten | WC20 | CeO2 | 1.80~2.20 | <0.2 | Remainder | tungsten | WZr3 | ZrO2 | 0.20~0.40 | <0.2 | Remainder | tungsten | WZr8 | ZrO2 | 0.70~0.90 | <0.2 | Remainder | tungsten | WP | ¡ª¡ª | ¡ª¡ª | <0.2 | 99.8 | tungsten | WY20 | Y2O3 | 1.80~2.20% | <0.2 | Remainder | tungsten
|
|
|